02 Reference
Defects and testing
Causes of defects, GOST, laboratory, acceptance
21articles
- 02 · Defects and testingWhy a slate sheet delaminates and how to find the causeA sheet delaminates when the layers built up on the format drum did not bond to each other. Look for the cause along the path of the sheet: slurry, screen, felt, vacuum, drum pressure and press, curing, demolding. Most often the culprits are a film that is too wet or too dry, a clogged felt and weak compaction.
- 02 · Defects and testingFlat sheet warps and bends: moisture and curingA flat sheet warps when one side dries or gets wet differently from the other: the wet side is longer, the dry side shorter, and the sheet bows. The causes are uneven moisture through the thickness, uneven laying in the stack and drying from one side. GOST 18124-2012 limits warping, and the allowance is larger for unpressed sheets.
- 02 · Defects and testingGOST 18124-2012: requirements for flat sheetsGOST 18124-2012 is the interstate standard for flat chrysotile-cement sheets. It divides sheets into pressed (LPP) and unpressed (LPN) and sets dimensions, flatness, bending strength, density, impact toughness and frost resistance. Amendment No. 1, in force from 1 January 2019, requires every sheet to be marked or to carry a label.
- 02 · Defects and testingA minimal slate plant laboratory: what it must haveA slate plant laboratory needs two parts. The first checks the finished sheet to GOST: a bending and load testing machine, a pendulum impact tester, a drying oven, scales with a hydrostatic weighing fixture, a freezer and measuring tools. The second watches the raw materials and the mass: cement, fibre opening or refining, concentration. Periodic tests can be given to an outside laboratory; acceptance tests are better done in house.
- 02 · Defects and testingEN 494 and ISO 10904: when you need them instead of GOSTEN 494 is the European standard for fibre-cement profiled sheets, ISO 10904:2011 the international one; ISO 9933 was withdrawn in 2011 and replaced by ISO 10904. Both describe asbestos-free sheets and test them differently from GOST: classes by profile height, breaking load and bending moment, and ageing tests. They are asked for in exports outside the CIS and in projects where the client works to European or international norms.
- 02 · Defects and testingHow a lot of slate is accepted: sampling and retestingA lot of slate is the shift output of one line. Every lot goes through acceptance tests: appearance, dimensions, load or bending, density. The other indicators are checked periodically. Sheets for checking are taken from different stacks, leaving out the outer ones. If the defects fall between the acceptance number and the rejection number, a second sample is taken. If a periodic test fails, control is switched to every lot.
- 02 · Defects and testingIs a certificate needed to sell slate in UzbekistanThe answer depends on the current list of objects subject to mandatory conformity confirmation (Cabinet of Ministers Resolution No. 43 of 30.01.2021) and on the HS code under which the sheet clears. The old 2011 list, which had products of cement and asbestos cement, lost force on 1 May 2021. Since 2026 a reform of technical regulation has been under way and the lists are changing. Check for your own sheet and for the current date.
- 02 · Defects and testingSelling slate in Kazakhstan and Kyrgyzstan: which documents are neededIn Kazakhstan slate falls under the national technical regulation on the safety of building materials (order No. 435 of 09.06.2023, in force since 19.12.2023). Asbestos-free corrugated sheets are in its mandatory certification list. There is no general EAEU regulation for building materials yet; it is being drafted. In Kyrgyzstan the 2010 national building materials regulation lost force in 2015; what is required now must be asked of the country's authority.
- 02 · Defects and testingA buyer complains about slate: how to work through the claimA claim is worked through in order: lot number and quality document, photos and the place of the defect, how the sheet was stored, transported and fastened, then sampling and testing to GOST. Under GOST 30340-2012 the manufacturer is responsible for the sheet conforming to the standard if the buyer observed the rules of transport, storage and use. The aim of the review is to tell a production defect from an installation error and to find the cause in both cases.
- 02 · Defects and testingVerifying scales and instruments at a slate plant: law and GOSTA sheet test result is worth as much as the instrument it was obtained with. GOST 30340-2012 sets the accuracy of the scales, the caliper and the bending testing machine. The Uzbek law "On Metrology" names the areas where measurements are under state control: accounting of material assets, industrial safety, quality of certified products, conformity assessment. Instruments for such measurements are, as a general rule, verified; where the law allows calibration instead of verification, check with the metrology service.
- 02 · Defects and testingWhere cracks in slate sheets come from: demolding, stack, roofFirst tie the crack to a time: did it appear right after demolding, in the stack in the finished goods warehouse, or already on the roof. That decides where to look for the cause: forming and curing, drying of the stack, or installation and frost.
- 02 · Defects and testingSheet thickness varies across or along: what has gone wrongThickness that varies across the width of the sheet almost always comes from an uneven layer building up on the screen or felt: a clogged screen, a skewed or worn felt, uneven vacuum across the width. Thickness that varies along the length and from sheet to sheet comes from slurry concentration and the number of turns on the format drum.
- 02 · Defects and testingFelt or screen marks on the sheet surface: defect or normalA light, even felt pattern on the underside of a corrugated sheet is normal: under GOST the back of the sheet is by definition the surface with felt or mesh imprints. The mark becomes a defect when it is sharp and uneven: a stripe from the seam, the imprint of a coarse yarn, patches from clogged areas. Then it points to a worn or greasy felt, wrong tension or wrong squeezing.
- 02 · Defects and testingWhite deposit on slate sheets: a defect or notThe white deposit is efflorescence: soluble calcium salts come out to the surface with water and turn into calcium carbonate there. It usually does not affect the strength of the sheet and is a defect of appearance only. But for a painted sheet the GOST does not allow efflorescence, and under the paint it spoils the coating.
- 02 · Defects and testingSlate lets water through: watertightness and water absorptionWatertightness is whether water passes through the sheet: under the GOST a column of water is placed on the sheet and after a day the underside is checked for drops. Water absorption is how much water the sheet soaks up; the GOST does not set a limit for it but gives a method. A porous sheet that soaks up a lot of water and lets it through most often has too little cement, weak compaction or early curing.
- 02 · Defects and testingHow slate is tested: bending, density, water absorption, frostSlate is checked for bending strength and strength under load, for density, impact toughness, water tightness, water absorption and frost resistance. The methods for corrugated sheets are now in GOST 30340-2012, for flat sheets in GOST 18124-2012; before that they were in GOST 8747-88. Each test answers its own question about the sheet, and each has its own specimen preparation.
- 02 · Defects and testingMarking slate and lots: what to write on the sheet and in the documentA corrugated sheet to GOST 30340-2012 is marked with the manufacturer (trademark or name), profile, thickness and lot number, on the face of the overlapped part. The OTK quality control stamp goes on at least 1 % of the sheets in a lot. A flat sheet to GOST 18124-2012, after Amendment No. 1, is marked on every sheet or carries a label. Every delivery is accompanied by a quality document with the test results of the lot.
- 02 · Defects and testingSheet breaks on impact and laying: why the strength is lowFour things set the bending and impact strength of a sheet: the fibre (how much there is and how it was opened or refined), the cement, the compaction of the layers and the curing. To find out which of them failed, compare the density and strength of the sheet with the norm and look at the fracture: a loose fracture means slurry and compaction, a dense but brittle one means fibre and curing mode.
- 02 · Defects and testingCrooked wave and uneven edge: which deviations are allowedFor a corrugated sheet the GOST measures length, width, thickness, wave height, deviation from squareness and straightness of the edges. The wave pitch is given for reference and is not a rejection criterion. A crooked wave usually comes from the templates and the corrugating machine, a skewed sheet and a ragged edge come from cutting.
- 02 · Defects and testingSlate crumbles after winter: what frost resistance meansFrost resistance is the number of freeze-thaw cycles in the wet state that a sheet withstands without delamination and without a large loss of strength. A sheet that takes up a lot of water crumbles after winter: the water in the pores freezes, expands and tears the stone. So in production frost resistance is above all density and low water absorption.
- 02 · Defects and testingGOST 30340-2012: what it requires of a corrugated sheetGOST 30340-2012 is the interstate standard for corrugated chrysotile-cement sheets and their fittings. It sets two profiles, dimensions and tolerances, strength, density, impact toughness, water tightness and frost resistance, and requirements for appearance, marking, acceptance and storage. It replaced GOST 30340-95 and, for corrugated sheets, GOST 8747-88 and GOST 30301-95.
Request