03 Reference
Slate technology
Slurry, forming, pressing, curing, autoclave
15articles
- 03 · Slate technologyAutoclave or air curing: which to choose for the sheetThe choice between an autoclave and curing in air is a choice of mix composition, not only of equipment. The autoclave gives fast strength gain and lets ground sand replace part of the cement, but it needs steam, a boiler and a pressure vessel. A mix with PVA fibre does not survive the autoclave; it is cured in air.
- 03 · Slate technologyThe Hatschek process in plain words: how a sheet is made from slurryIn the Hatschek process the sheet is built from many thin films. A mesh cylinder in a vat of liquid slurry filters out the water and leaves a film on the screen, the felt lifts it off and carries it over the vacuum to the format drum, and the drum winds it on layer after layer to the required thickness. Then the wrap is cut open, the sheet is corrugated or left flat, and sent to curing.
- 03 · Slate technologySlurry concentration in the vat: why it sets thickness and strengthConcentration is how much solid (cement, fibre, filler) there is in the water of the vat. It decides what film lies on the screen in one turn: a thicker slurry gives a thicker, denser film, a thinner one a thinner film. If the concentration wanders, the sheets come out with different thickness and different strength. It is held constant: recycled water is added by measurement, and measurements are taken regularly.
- 03 · Slate technologyWhy slate is pressed and how the press affects strengthThe press squeezes the raw sheet further after forming: it forces out water, brings the layers and fibres closer and removes some of the pores. A pressed sheet is denser, stronger, holds frost and water better and is flatter. That is why the interstate standard for flat sheets divides them into pressed and unpressed ones with different requirements. Corrugated slate is usually not pressed; the press is needed first of all for flat sheet and higher-grade products.
- 03 · Slate technologyPre-curing: when a sheet can be taken off its templateAfter forming, a raw sheet is soft, like wet cardboard. While it lies on its template or pallet in the chamber, the cement sets and the sheet gains demolding strength: enough to be taken off, turned over, trimmed and stacked without cracks. Time and temperature are not guessed: they are set by the regulations, and readiness is checked on a control sheet. A sheet taken off too early cracks and breaks later, in the warehouse and on the roof.
- 03 · Slate technologyFlat fibre-cement sheet: how the technology differs from slateA flat sheet is formed the same way as slate, on a Hatschek machine. The differences start after the format drum: no corrugating, but often a press; the sheet hardens on flat pallets or in an autoclave; the requirements for flatness, the face and the edge are stricter. The main defects of a flat sheet are warping and marks on the face, which are almost unnoticeable on a corrugated sheet.
- 03 · Slate technologyTrimming and cutting slate to size: wet, dry and offcutsSlate is cut twice. The raw wrap is cut into blanks and the edges trimmed while the sheet is soft: with shears, disc knives or a water jet. The hardened sheet is cut when an exact size or a clean edge is needed: with a saw or abrasive waterjet, and then dust appears. Raw offcuts go straight back into the slurry through the agitator. Hardened offcuts cannot be returned to ordinary slurry: they are either ground to powder as a filler or taken away under the rules of the country.
- 03 · Slate technologyBatchers and scales: why mix accuracy decides defectsA slate sheet depends on the ratio of cement, fibre and water. If the cement or fibre scales lie, the slurry composition changes from batch to batch, and it shows on the sheet: sometimes brittle, sometimes loose, sometimes of uneven thickness. So the scales are checked with test weights, the load cells and indicator are kept in order, and the flow of water and pulp is checked against the regulations.
- 03 · Slate technologyAutoclave at a slate plant: what it is for and what gets servicedAn autoclave is needed where the mix contains ground quartz sand: under saturated steam pressure the sand reacts with the lime from the cement, and the sheet gains strength in a single cycle. What wears out in it: the seal of the quick-opening lid and its mechanism, steam traps and drainage, valves and safety valves, rails and cars. In Uzbekistan the autoclave is pressure equipment and falls under technical regulation CMR No. 493.
- 03 · Slate technologyCuring chambers: temperature, humidity and where rejects come fromIn the curing chamber the green sheet gains the strength to be taken off the pallet without breaking. Three things cause rejects here: heat applied before the cement began to set; temperature raised too fast or unevenly; the sheet losing water to dry air and drafts.
- 03 · Slate technologyWhere a slate plant needs steam and how not to lose it on the wayAt a slate plant steam goes to the autoclave, to the curing chambers and, in winter, to heating water and buildings. It is lost on the way in three places: bare pipes and valves without insulation, faulty steam traps, and condensate drained into a ditch instead of returned to the boiler house.
- 03 · Slate technologyCan flat sheet be made on a corrugated slate lineIt can: flat and corrugated sheet are formed in the same way, on the same Hatschek machine. A corrugated sheet is made from a flat blank on a corrugator, and a flat sheet bypasses it. But a marketable flat sheet usually needs sections that a corrugated line lacks or has only weak ones: a press, flat pallets, and for facade boards an autoclave, drying, sanding and painting.
- 03 · Slate technologyHow much vacuum a sheet needs, and what too little or too much doesThe vacuum under the felt sucks water out of the film before it reaches the format drum. Too little vacuum and the film arrives wet, the layers press together poorly, and the sheet slumps and delaminates. Too much and the film dries out and bonds worse with the next layer, and the felt wears and clogs faster. There is no single number for all lines: the vacuum level is set by the regulations and watched by the gauge and by the sheet.
- 03 · Slate technologyHow slate gets its wave and why the profile comes out unevenThe wave is given to the raw flat sheet right after the wrap is cut, while it is still soft. The corrugator (rod, chain or vacuum type) bends the sheet to the profile, then the sheet is laid on a corrugated spacer or in a profiled cart and held in that shape until it hardens. An uneven wave almost always comes from three places: sheet moisture and thickness, wear of the corrugator, and the condition of the templates and carts.
- 03 · Slate technologyPainting slate: which paint and at what stageAt the plant, slate is painted in two ways: on the fresh, not yet hardened sheet, or on the hardened one. A fresh sheet is painted so that the paint also blocks the path of efflorescence, which comes out just as the cement hardens. A hardened sheet is simpler to paint in terms of process, but efflorescence and dust must be removed before painting. Most often acrylic water-based dispersions designed for a cement substrate are used; silicate compositions less often. Colour, evenness and abrasion resistance of the coating are checked to GOST.