0In the list
02Defects and testing

Slate crumbles after winter: what frost resistance means

Frost resistance is the number of freeze-thaw cycles in the wet state that a sheet withstands without delamination and without a large loss of strength. A sheet that takes up a lot of water crumbles after winter: the water in the pores freezes, expands and tears the stone. So in production frost resistance is above all density and low water absorption.

Updated 5 min read

In short

5minutes to read

7sections

5sources

3catalog items

In this article

  1. 01What the standard requires
  2. 02Why the sheet is destroyed
  3. 03How it is tested
  4. 04What raises frost resistance in production
  5. 05What is down to the roof and not the plant
Contents
  1. What the standard requires
  2. Why the sheet is destroyed
  3. How it is tested
  4. What raises frost resistance in production
  5. What is down to the roof and not the plant
  6. How to handle a complaint
  7. How we do it

Frost resistance is the number of freeze-thaw cycles in a water-saturated state that a sheet withstands without delamination and without a noticeable loss of strength. If slate flakes, delaminates and crumbles after winter, it means it takes up too much water. The water in the pores freezes, expands and tears the cement stone from inside, cycle after cycle. So in production frost resistance rests on the same things as watertightness: density, a good bond between layers, correct curing. It is checked under the GOST by a periodic test.

What the standard requires

Corrugated sheets. GOST 30340-2012 sets a minimum number of cycles. After them the specimens must show no delamination, and the bending strength must stay almost at its original level. The test is periodic and is carried out at least as often as the standard sets.

Flat sheets. In GOST 18124-2012 the number of cycles for pressed sheets is greater than for unpressed ones. Compaction directly affects resistance to frost.

EN 494. In the European standard for profiled sheets the freeze-thaw test is longer. The result is expressed as the share of strength retained. Manufacturers state it in their declarations.

Take the number of cycles and the permitted loss of strength for your product from the current edition of the standard. The figures of the GOST and EN are not compared directly: the methods differ.

Why the sheet is destroyed

Water increases in volume when it freezes. If it fills the pores almost completely, it has nowhere to expand and presses on the pore walls. Microcracks appear. On thawing, the water goes deeper into them, and at the next frost it presses again. This is how the sheet loses strength gradually.

Reference books on building materials name the main factor: the more pores in the material that are accessible to water, the lower the frost resistance. The pore structure matters too: small closed pores do less harm than open capillaries. Hence the ways to raise frost resistance: reduce water absorption, compact the material, reduce the share of open pores.

A layered sheet has one more weak spot: the boundary between layers. If the layers are poorly bonded, water collects between them, and frost splits the sheet. That is why the standard checks for delamination after the cycles.

How it is tested

The essence of the method under GOST 30340-2012:

  1. Two specimens are cut from each selected sheet: a main one and a control one.
  2. The main specimens are saturated with water.
  3. They are frozen in a freezer and thawed in water. The temperature and time of each stage are set by the standard.
  4. After the set number of cycles they are examined for delamination.
  5. The main and control specimens are saturated with water again and tested in bending.
  6. The ratio of the average strength of the main specimens to the average strength of the control ones is the residual strength.

The test needs a freezer, a thawing bath and a machine for bending tests. If the plant does not have them, the test is ordered from an accredited laboratory.

What raises frost resistance in production

  • Density. Compaction on the format drum and in the press. A press that does not hold pressure at once lowers frost resistance.
  • Cement. A sufficient share of cement fills the pores between the fibres.
  • Bond between layers. Everything that causes delamination: a wet or over-dried layer, a clogged felt, weak pressing.
  • Fibre. Good opening of the asbestos, correct refining of the cellulose. Loose clumps of fibre are ready-made channels for water.
  • Curing. A sheet that dried out before gaining strength comes out porous. On an autoclave line the autoclave mode matters.
  • Painting. The coating on the face side reduces the soaking of water from above. But if it cracks and peels, water gets under it.

What is down to the roof and not the plant

A sheet on a roof gets wetter if water stands on it for a long time: a low slope, snow at the eave, clogged gutters, an underside without ventilation. This does not remove the question to the plant, but it explains why on one roof sheets from the same lot stand and on another they crumble.

How to handle a complaint

  1. Find the lot number from the marking.
  2. Check the results of the periodic frost resistance test for that period.
  3. If the test was not done for a long time, test archive or new sheets.
  4. Compare the water absorption and density of sheets from this lot with good ones.
  5. See where the destruction is on the roof: over the whole sheet or in places where water stands.

How we do it

  • From the photo, dimensions and the passport of the unit, we look for the item at the manufacturing plant. What we find, with the price, photos and specifications, we send before the order.
  • We inspect the lot at the plant before shipment: part number, dimensions, lot, packaging.

What this article relies on

Below are the documents and materials we refer to, so that you can check what is said for yourself.

Standards and documents

  • GOST 30340-2012 "Chrysotile-cement corrugated sheets. Specifications": frost resistance requirement, test method, frequencytext ↗
  • GOST 18124-2012 "Chrysotile-cement flat sheets. Specifications": frost resistance of pressed and unpressed sheets, residual strengthtext ↗

Reference materials

  • Great Russian Encyclopedia (Большая российская энциклопедия), article "Frost resistance": dependence on the volume of pores accessible to water, ways of raising itbigenc.ru ↗
  • "Physical and mathematical modelling of frost resistance of cement concretes" (Физико-математическое моделирование морозостойкости цементных бетонов), journal "Structural Mechanics of Engineering Constructions and Buildings" (RUDN University): critical water saturation and formation of defects during cyclesjournals.rudn.ru ↗
  • Declaration and technical data of profiled sheets to EN 494 (Eternit Baltic): freeze-thaw test, share of strength retainedtaloon.com ↗

The test modes follow the text of the current standard; the production modes follow the process regulations of your line.

Related catalog items

  • 001Hydraulic press 3000–15000 t

    Hydraulic press 3000–15000 t

    TMN-XHB-02Xinhuibo

  • 002Autoclave for fiber-cement sheet

    Autoclave for fiber-cement sheet

    TMN-XHB-03Xinhuibo

  • 003Disc refiner for pulp

    Disc refiner for pulp

    TMN-XHB-12Xinhuibo

For slate plants

Felts, meshes and units for your line

We select from manufacturing plants in China by nameplate photo and machine dimensions. Send a photo of the plate and we will tell you what can be ordered.

Request

Ask about your machine

A part number is enough. A drawing or a photo of the unit speeds up sourcing but is not required.

Up to 3 files: photos (JPG, PNG, WEBP, HEIC) or PDF, up to 15 MB in total

By sending the request you consent to the processing of the data provided for the purpose of replying to it, as described in the Privacy Policy.