Felt or screen marks on the sheet surface: defect or normal

A light, even felt pattern on the underside of a corrugated sheet is normal: under GOST the back of the sheet is by definition the surface with felt or mesh imprints. The mark becomes a defect when it is sharp and uneven: a stripe from the seam, the imprint of a coarse yarn, patches from clogged areas. Then it points to a worn or greasy felt, wrong tension or wrong squeezing.

Updated 5 min read

In short

5minutes to read

7sections

4sources

4catalog items

In this article

  1. 01What the standard says
  2. 02Why the felt leaves a mark at all
  3. 03What the marks point to
  4. 04Link to screen marks
  5. 05When to change the felt
TableWhat the marks point to6 rows →
Contents
  1. What the standard says
  2. Why the felt leaves a mark at all
  3. What the marks point to
  4. Link to screen marks
  5. When to change the felt
  6. What to tell us when ordering a new felt
  7. How we do it

The felt pattern on the surface of a sheet is not a defect in itself. For a corrugated roofing sheet a light, even imprint is normal, and for some products it is even sought on purpose: the relief helps the layers to bond. The mark becomes a defect when it is uneven and sharp. That means a stripe across the sheet from a seam, a coarse imprint of individual yarns, patches where the felt has clogged or worn through. Such a mark tells you about the condition of the felt. Usually it is wear, greasing, wrong tension or wrong squeezing. If the sheet is later painted or sold as a facing sheet, the requirements for the surface are stricter.

What the standard says

GOST 30340-2012 for corrugated sheets classes roughness and imprints from metal process pads as insignificant defects, that is, it allows them. And the standard directly defines the back (non-face) side as the surface bearing imprints of the felt or mesh; the face side has none. Other things are limited: scuffs, chips, surface breaks, unevenness in height. For painted sheets the requirements are stricter: the coating must be even, without patches visible from a distance. A pattern that shows through the paint in patches or stripes is already questionable.

Flat sheets, especially those pressed for cladding, are judged more strictly. There the buyer looks at the face side.

The practical conclusion for the plant: agree with quality control and with buyers on which pattern counts as normal for each product. It is best to keep a reference sheet.

Why the felt leaves a mark at all

The felt in a Hatschek machine is a woven base with a batt of synthetic fibre laid on top. The layer of slurry lies on the batt, the felt carries it over the vacuum boxes and presses against the format drum. Whatever is on the surface of the felt is imprinted on the green layer: the weave, the pile, the seam, stuck-on lumps.

Patents on felts for fibre cement describe this directly:

  • some felts are made "marking" on purpose: they leave a relief on the sheet so that the next layer bonds better. Such felts are used for roofing and corrugated sheets and pipes;
  • marking felts lose their ability to mark over time, because the fabric gets dirty;
  • felts with coarse yarns can press into the surface so hard that the sheet then has to be smoothed. That is why felts with fine top yarns are made for smooth products.

From this comes the first rule: choose the felt for the product. A felt for corrugated sheet may not suit a smooth flat sheet.

What the marks point to

What you see on the sheetLikely causeWhat to check
Even fine pattern over the whole areanormal work of the feltnothing, if the product allows it
Cross stripe at regular intervalsseam of the endless feltcondition of the seam, joining method, tension
Imprint of individual coarse yarnsbatt worn, base exposedinspect the felt; if the batt is worn off, replace
Patches, "clouds", places with no patternfelt clogged in areaswashing, sprays, vacuum
Lengthwise stripesfold, felt running off, uneven tension across the widthtension, tracking correction, wear of rolls
Lumps and dentsslurry stuck to the felt or drumwashing, scrapers

This is a scheme for searching. The process engineer determines the final cause by inspecting the felt.

Link to screen marks

The pattern of the cylinder screen may also be visible on the sheet. It is finer and is usually smoothed out by the felt. If the screen pattern shows through sharply or with holes, the screen is torn, dented or unevenly clogged. It is checked separately.

When to change the felt

A mark is one of the signs that the felt is due for replacement. The others: the felt gives up water worse, has stretched and runs off, is torn, the batt is peeling off. Service life depends on the slurry, machine speed, washing and tension. There is no general figure.

If the felt is still intact but the mark has appeared, first check:

  1. washing and sprays: a greasy fabric can often be brought back;
  2. tension: weak tension gives folds, too strong wears out and stretches the felt faster;
  3. squeeze rolls: uneven squeezing gives lengthwise stripes;
  4. the seam: on felts with a seam, the joint wears out before the fabric.

What to tell us when ordering a new felt

  1. The product: corrugated sheet, flat, for painting or not.
  2. The slurry: asbestos cement or fibre cement.
  3. The fabric type and density of the old felt, its tag and part number.
  4. The size from the machine's passport, endless or seamed.
  5. A photo of the mark on the sheet and photos of the old felt from both sides.

With a photo of the mark it is easier to explain the task to the manufacturer: whether a finer batt is needed or a base with a different weave.

How we do it

  • From the tag, photo and dimensions of the old felt, we look for the item at the manufacturer. What we find, with the price, photos and specifications, we send before the order.
  • We inspect the lot at the plant before shipment: part number, dimensions, lot, packaging.

What this article relies on

Below are the documents and materials we refer to, so that you can check what is said for yourself.

Standards and documents

  • GOST 30340-2012 "Chrysotile-cement corrugated sheets. Specifications": permitted insignificant surface defects, requirements for painted sheetstext ↗

Reference materials

  • Patent US 9415564 "Felt for forming fiber cement articles and related methods": marking felts, contamination and loss of markingpatents.google.com ↗
  • Application US 2005/0085148 "Felt for forming fiber cement articles with multiplex base fabric": coarse yarns press into the surface of the sheet, felts with fine top yarnspatents.justia.com ↗
  • taminota.com catalog: forming and needle-punched felts TMN-XHB-F01 to F05, fabric type and purpose per the manufacturer's data.

The "mark and cause" table is drawn up from the design of the felt and the machine, without a separate external source.

Related catalog items

  • 001

    Asbestos-cement forming felt 94047 · 1700 g/m²

    TMN-XHB-F01Xinhuibo

  • 002

    Fiber-cement forming felt 94047-1 · 1650 g/m²

    TMN-XHB-F02Xinhuibo

  • 003

    Needle-punched forming felt 51291 · 1000 g/m²

    TMN-XHB-F03Xinhuibo

  • 004

    Synthetic fiber forming felt 97049 · 1800 g/m²

    TMN-XHB-F04Xinhuibo

For slate plants

Felts, meshes and units for your line

We select from manufacturing plants in China by nameplate photo and machine dimensions. Send a photo of the plate and we will tell you what can be ordered.

Request

Ask about your machine

A part number is enough. A drawing or a photo of the unit speeds up sourcing but is not required.

Up to 3 files: photos (JPG, PNG, WEBP, HEIC) or PDF, up to 15 MB in total

By sending the request you consent to the processing of the data provided for the purpose of replying to it, as described in the Privacy Policy.