Felts and meshXinhuibo
Needle-punched forming felt 51291 · 1000 g/m²
Basis weight1000г/м²
- TAMINOTA part number
- TMN-XHB-F03
- Manufacturer part number
- 51291
A needle-punched asbestos cement felt for forming sheet. High strength in the warp, good dewatering.
- Brand
- Xinhuibo
- Category
- Felts and mesh
- Industry
- Asbestos and fiber cement
- Availability
- Made to order
What to send for selection
- 01Machine model and forming method
- 02Slurry: asbestos cement or fiber cement
- 03Belt length under tension and width — from the machine passport or a previous order
- 04Joint: endless or seamed
- 05Photos of the machine nameplate and the old felt
Specifications
TMN-XHB-F03
- Type
- Иглопробивное
- Purpose
- Шифер
Dimensions for ordering
- Basis weight
- 1000 г/м²
- Width
- confirmed from your machine dimensions
- Belt length
- confirmed from your machine dimensions
- Thickness
- confirmed from your machine dimensions
- Air permeability
- confirmed from your machine dimensions
How to get this item
- 01You send the part number or a nameplate photo
- 02You get the plant’s invoice and a lead time
- 03Inspection at the plant, delivery, documents
Related articles
- Forming felt for sheet lines: how to choose and when to changeChoose the felt by the slurry the machine runs on (asbestos cement or fibre cement), the type of fabric (woven or needle-punched), the density in g/m² and the exact width and length of your machine. Change it when it clogs and drains poorly, stretches or starts to mark the sheet.
- Why forming felt clogs fast and how to make it last longerThe felt on a sheet machine is clogged by cement and fines from the slurry; this is unavoidable. It clogs fast when washing cannot cope, when the slurry is not what it should be, or when the felt does not suit the slurry. Its life is extended by sprays, suction, correct tension and a stable slurry, not only by changing the supplier.
- Fitting a new felt on the machine without ruining it in the first daysA new felt goes onto a clean machine with checked rolls, doctors and sprays, strictly along the direction arrow. Tension it gradually, bring it up to speed with water and only then feed slurry. A new felt is ruined by skew, dirt on the rolls, sudden tension, a dry start and knocks against the edge.
- Forming machine spare parts to keep in stock for a yearFor a Hatschek machine keep in stock what is made to your machine's size and what stops it when missing: felts, cylinder screens, vacuum box strips, knives, coverings and roll bearings, pump impellers and liners, spray nozzles. Work out the quantity from your own replacement log, not from someone else's norm.
- How to measure a forming felt and cylinder screen for an orderTo order a felt you need the length of the closed loop under working tension, the width, the joint type (endless or seamed), the fabric type and density, the slurry and the machine. Take the length from the machine passport or a previous order; if you measure on the machine, use a non-stretch cord with the tensioner at mid-travel, never the old felt lying on the floor.
- g/m², air permeability, thickness: how to read a felt specificationThe main lines in a felt specification are density in g/m², thickness, air permeability, tensile strength and elongation, material and fabric type. Density and material can be compared between plants directly. Thickness and air permeability can be compared only if they were measured the same way: under the same load, the same pressure drop and in the same units.
- How to trial a felt from another maker without risking outputA new felt is trialed on one machine, with a proven felt in reserve nearby. Before installation, record how your current felts perform; during the trial, record vacuum, sheet thickness and moisture, marks on the sheet, washes and the day of removal. Compare felts of the same age. One trial felt shows whether the fabric suits your machine at all, but does not prove the whole lot will be the same.
- When to order spare parts so you do not stand in the seasonCount from the date the part must be in your hands: the start of the repair shutdown or the start of the sales season. From it subtract the production time, transport, customs and a reserve for the unexpected — that gives the last order day for each item. Felts, screens, parts to drawing and large bearings are ordered first; off-the-shelf consumables last.
- Why a spare felt spoils on the shelf and how to store itFelts are made mainly of polyamide (nylon). In light it loses strength, with moisture it changes size, and under a load or at folds the fabric creases and cakes. So spare felt is kept in the factory packaging, in a dry dark room, off the floor, with no load on top and no folds, with a lot label and date, and the earlier arrival goes on the machine first.
- How to choose a felt and screen supplier: what to ask before orderingBefore ordering, find out five things: whether the supplier makes the felts himself or resells them; on what slurries and machines his felts already work; whether there is a data sheet with the test methods; how he keeps lots uniform; how he handles a claim. Then one trial felt on your machine, and only after that a stock.
- Why a slate sheet delaminates and how to find the causeA sheet delaminates when the layers built up on the format drum did not bond to each other. Look for the cause along the path of the sheet: slurry, screen, felt, vacuum, drum pressure and press, curing, demolding. Most often the culprits are a film that is too wet or too dry, a clogged felt and weak compaction.
- Sheet thickness varies across or along: what has gone wrongThickness that varies across the width of the sheet almost always comes from an uneven layer building up on the screen or felt: a clogged screen, a skewed or worn felt, uneven vacuum across the width. Thickness that varies along the length and from sheet to sheet comes from slurry concentration and the number of turns on the format drum.
- Felt or screen marks on the sheet surface: defect or normalA light, even felt pattern on the underside of a corrugated sheet is normal: under GOST the back of the sheet is by definition the surface with felt or mesh imprints. The mark becomes a defect when it is sharp and uneven: a stripe from the seam, the imprint of a coarse yarn, patches from clogged areas. Then it points to a worn or greasy felt, wrong tension or wrong squeezing.
- GOST 30340-2012: what it requires of a corrugated sheetGOST 30340-2012 is the interstate standard for corrugated chrysotile-cement sheets and their fittings. It sets two profiles, dimensions and tolerances, strength, density, impact toughness, water tightness and frost resistance, and requirements for appearance, marking, acceptance and storage. It replaced GOST 30340-95 and, for corrugated sheets, GOST 8747-88 and GOST 30301-95.
- How slate is tested: bending, density, water absorption, frostSlate is checked for bending strength and strength under load, for density, impact toughness, water tightness, water absorption and frost resistance. The methods for corrugated sheets are now in GOST 30340-2012, for flat sheets in GOST 18124-2012; before that they were in GOST 8747-88. Each test answers its own question about the sheet, and each has its own specimen preparation.
- A buyer complains about slate: how to work through the claimA claim is worked through in order: lot number and quality document, photos and the place of the defect, how the sheet was stored, transported and fastened, then sampling and testing to GOST. Under GOST 30340-2012 the manufacturer is responsible for the sheet conforming to the standard if the buyer observed the rules of transport, storage and use. The aim of the review is to tell a production defect from an installation error and to find the cause in both cases.
- Starting a new line: what goes wrong in the first weeksIn the first weeks a new line almost always gives less sheet and more rejects than promised: the slurry and felts are not yet matched to your raw materials and water, the shifts are learning, the units are running in, small installation flaws surface one after another. This is normal if every stoppage and every kind of reject is recorded: these records are needed both for tuning and for the warranty.
Request
Send a part number or a photo — we will find the factory
Items from the catalog · 1
- TMN-XHB-F03 · Needle-punched forming felt 51291 · 1000 g/m²