Cylinder mould screen: which mesh to fit and when to replace it
The screen decides how much fibre and cement stays on the cylinder and how much leaves with the water. Choose the mesh by the slurry (asbestos cement or fibre cement), by its number (meshes per inch) and by the wire material. Replace it by condition: clogged, torn, sagging or giving an uneven layer.
In short
5minutes to read
7sections
4sources
1catalog item
In this article
Contents
The screen of a cylinder mould is chosen by three things: what slurry the machine runs on, which mesh number is needed and what wire the mesh is made of. The number is the count of meshes per inch: the higher it is, the finer the opening and the slower the water drains. It is time to replace the screen when it has clogged and washing no longer helps, when tears and dents have appeared, or when the layer on the cylinder lies unevenly. The screen is made to the diameter and length of your cylinder, so keep a spare in advance.
What the screen does
In the vat of a Hatschek machine, a hollow cylinder covered with mesh rotates. It is half submerged in diluted slurry. Water passes through the mesh to the inside of the cylinder and drains away at the end. Fibre and cement stay on the surface as a thin film. The felt presses against the cylinder from above and lifts this film off. After that the mesh is washed with a spray, and the water runs back into the vat.
So the screen works as a filter. Fibres lie on the openings and themselves form a web that holds the fine cement particles. If the opening is too coarse, the fines leave with the water, and the film comes out thin and loose. If it is too fine, the water drains slowly and the cylinder does not have time to pick up a layer.
How the mesh on the cylinder is built
A cylinder usually carries two meshes. Underneath is the backing mesh, coarse: it holds the shape and gives the water a path inward. On top is the face mesh, fine: the layer builds up on it. In papermaking, where this design comes from, the backing mesh is around 8–16 meshes per inch and the face mesh around 50–80. Both are stretched over the cylinder and fixed at the edges by soldering.
This is why replacing the face mesh is not an hour's job. The old one is removed, the ends are cleaned, and the new one is stretched evenly, without waves or skew. A badly stretched mesh sags between the bars of the frame, and the layer lies thicker at that spot.
Which number to choose
The answer depends on the slurry.
- Asbestos cement. Chrysotile fibre is thin and holds cement well. In patent descriptions of the Hatschek machine, a mesh of 40–50 meshes per inch is named as usual for such a slurry.
- Asbestos-free fibre cement. Cellulose and synthetic fibres hold cement less well, and water drains faster. One patent on asbestos-free sheet reports that a mesh of about 70 meshes per inch gave a better layer because it slowed the drainage. Another patent stresses the role of cellulose: it is the first to lie on the wire and then works as a filter for the rest of the slurry.
These are reference points from open descriptions, not a norm for your machine. If the plant has moved from asbestos cement to fibre cement, the mesh number is checked again together with the felt and the recipe. The best starting point is the mesh your machine already runs well on. Its number, wire and weave are worth writing in the log.
Bronze or stainless steel
The traditional material for cylinder meshes is phosphor bronze. It draws well, solders easily and does not rust in water. Stainless wire is stronger and resists abrasion better, but it is harder to solder and costs differently. Combined meshes exist too. The choice depends on what exactly kills the screen on your machine: abrasion by the slurry, corrosion in the process water, or mechanical knocks during cleaning. If the old mesh served well, it is reasonable to order the same wire.
When to replace
The life of a screen depends on the slurry, the process water, the sprays and the care taken in cleaning. There is no general figure. Signs that the screen is due for replacement:
- Clogging. Washing does not bring back the permeability, water stands on the mesh, the layer is thinner than usual.
- Tears and holes. Thickened spots or blotches appear on the sheet at the same place across the width.
- Dents and sagging. The mesh has sagged between the bars, and a stripe is visible on the sheet.
- Solder breaking away at the edge. The mesh lifts at the ends, the sheet edge tears.
- Uneven thickness across the width, if the felt and the vacuum are in order.
It is best to clean the screen during a stop with water and a soft brush. A scraper and hard tools leave dents that later show on the sheet.
What to tell us when ordering
- The diameter and length of the cylinder, the length of the working part.
- The number of the face and backing mesh, if known, and the weave.
- The wire material and its diameter.
- The slurry: asbestos cement or fibre cement, and which product.
- A close-up photo of the old mesh next to a ruler: it shows the opening and the wire.
- How the mesh is fixed to the cylinder: soldering, strips, a removable shell.
If the cylinder comes from a machine with no documents, we need a sketch with the dimensions of the ends and the frame.
How we do it
- From the dimensions, photos and passport of the old mesh, we look for the item at the manufacturing plant. What we find, with the price, photos and specifications, we send before the order. If the plant's designation is different, we say how the item differs.
- We inspect the lot at the plant before shipment: part number, dimensions, lot, packaging.
What this article relies on
Below are the documents and materials we refer to, so that you can check what is said for yourself.
Reference materials
- Patent US 4543159 "Reinforced cement sheet product containing no asbestos for fabricating on Hatschek machine": the design of the cylinder and vat, spray washing of the mesh, the usual 40–50 mesh and the trial with about 70 meshpatents.google.com ↗
- Patent US 6824715 "Method and apparatus for forming a laminated sheet material by spattering", background section: cylinder moulds, cellulose as a filtering layer on the wirepatents.google.com ↗
- Application EP 0902121 on cylinder moulds of paper machines: backing and face mesh, soldering at the ends, the difficulty of replacementdata.epo.org ↗
- Paper World, overview of cylinder moulds and their coverings for the paper and board industrypaper-world.com ↗
Mesh numbers are taken from patent descriptions and given as a reference point. The signs of wear are described from general operating practice.