St3sp · 09G2S · 15×15–300×300 · GOST 8639 · GOST 30245
Square hollow section
Closed square section for frames, trusses and fencing. Wall 1–12 mm, St3sp, 09G2S, Q235B, Q355B

St3sp · 09G2S · 20×10–300×200 · GOST 8645 · GOST 30245
Closed rectangular section for purlins, beams and frames. Wall 1–12 mm, St3sp, 09G2S, Q235B, Q355B
| Parameters | |
|---|---|
| Section | 20×10 – 300×200 mm |
| Wall thickness | 1.0–12 mm |
| Length | 6 and 12 m; fixed length to specification |
| Steel grade | St3sp, 09G2S; Q235B, Q355B per GB |
| Acceptance standard | GOST 8645 and GOST 13663; GOST 30245 for building structures |
| Weld | single, on the corner; outer weld bead removed |
| Size, mm | Weight, kg/m |
|---|---|
| 20×10×1.5 | 0.605 |
| 30×20×2 | 1.39 |
| 40×20×2 | 1.7 |
| 40×25×2 | 1.86 |
| 50×25×2 | 2.18 |
| 60×30×2 | 2.65 |
| 60×40×3 | 4.31 |
| 80×40×3 | 5.25 |
| 80×60×4 | 8.07 |
| 100×50×4 | 8.7 |
| 120×60×4 | 10.6 |
| 120×80×5 | 14.6 |
| 150×100×6 | 21.9 |
| 200×100×6 | 26.6 |
| 200×120×8 | 37.3 |
| 300×200×8 | 59.9 |
Theoretical weight at steel density 7.85 g/cm³. Actual batch weight is by scale and mill certificate.
A rectangular hollow section is a closed welded profile with two pairs of faces of different width. It is produced the same way as the square one: from a round welded pipe sized into a rectangle, or by direct forming of strip with a weld on one face. Size range to GOST 8645-68, technical requirements to GOST 13663-86, for building structures — GOST 30245-2003. At mills in China this is GB/T 6728-2017, for export ASTM A500/A500M and EN 10219-1. Because of the different height and width, the section gives a larger section modulus in the plane of the longer side than a square section of the same weight, so rectangular sections are used for purlins, beams and girders.
The grades are St2sp, St3sp and St3ps for fencing and light frames, 09G2S for load-bearing structures and service at sub-zero temperatures. At mills in China St3sp corresponds to Q235B, 09G2S to Q355B; export versions are S235JRH and S355J2H under EN 10219, A500 Gr.B and Gr.C under ASTM. The size designation is written as height × width × wall, and the order of sides matters in the specification: 60×40×3 and 40×60×3 are the same section, but when purlins are laid out the orientation of the section is set by the project. The acceptance standard is written separately: GOST 8645 sets the size range, GOST 30245 the mechanical properties and tolerances for structures.
During inspection at the mill, the height and width of the rectangular section are measured with callipers at the ends of the sampled lengths, the wall thickness with a micrometer on a flat face away from the weld. Concavity and convexity of the faces are checked, squareness of adjacent faces with a square, twist along the length, corner radius with a template, condition of the weld and ends. The heat number in the marking is matched against the mill test certificate (MTC): chemical composition and mechanical properties for sections to GOST 30245. The bundle tag and strapping are checked. Rejects recorded in the report are replaced; the replacement is supplied by the manufacturing mill under its contract with the bureau.
Rectangular bundles strapped with steel band; the bundle carries a mill tag with size, wall thickness, grade and heat number.
| GOST | GB (China) | ASTM | EN | Note |
|---|---|---|---|---|
| Steel 20 | 20# | A106 Gr.B | P235GH | Seamless pipes. Nearest equivalents by composition and strength; test requirements differ between the standards |
| Steel 45 | 45# | 1045 (A519) | C45 | Seamless pipes for machining, nearest equivalents. A519 is a standard for mechanical tubing; C45 under EN 10083 is a steel grade, tubes in it are made to EN 10297-1 |
| 09G2S | Q355B | A572 Gr.50 | S355J2H | Low-alloy steel, nearest equivalents. Before GB/T 1591-2018 the grade was designated Q345B; A572 is a standard for rolled products, not for pipe; S355J2H is a hollow section grade under EN 10219 |
| St3sp | Q235B | A53 Gr.B | P235TR1 | Welded pipes. A53 Gr.B is the nearest equivalent: its tensile strength is higher than that of Q235B |
| St3sp | Q235B | A500 Gr.B | S235JRH | Hollow sections. A500 specifies a higher yield strength than Q235B; structural design uses the standard stated in the specification |
| St2sp, St3sp | Q195, Q235 | A53 Gr.A | S195T | Water and gas pipes. GOST 3262 does not specify mechanical properties, so the grade comparison is nominal |
| K42 (GOST 20295) | L245 (GB/T 9711) | API 5L Gr.B | L245NB | Spiral-welded pipes. A strength class by tensile strength, not a steel grade |
| 08Kh18N10 | 06Cr19Ni10 | TP304 | 1.4301 | Stainless pipes. Austenitic 18-10 steel; 03Kh17N14M3 corresponds to TP316L and 1.4404 |
Equivalents are the closest match, not identical: chemistry and tolerances differ between standards. The exact grade and standard are written into the contract.

St3sp · 09G2S · 15×15–300×300 · GOST 8639 · GOST 30245
Closed square section for frames, trusses and fencing. Wall 1–12 mm, St3sp, 09G2S, Q235B, Q355B

St3sp · Q235B · Ø57–530 · GOST 10704
Round pipe from strip with a high-frequency weld. Structures, fencing, low-pressure water and gas
Price request
Steel pricing depends on grade, size, tonnage and delivery terms on the day of contract. A number on the page would be wrong by the time you read it.
Request received